PS Synthos PS HI 552M SYNTHOS POLAND
0
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 9.0 kJ/m² |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 120 kJ/m² |
| flammability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| UL flame retardant rating | 1.6mm | UL 94 | HB |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Vicat softening temperature | ISO 306/B50 | 88.0 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | 200°C/5.0kg | ISO 1133 | 9.0to10 g/10min |
| Shrinkage rate | Internal Method | 0.30to0.60 % | |
| Particle size distribution | 2.50to4.00 mm |
| Supplementary Information | Test Condition | Test Method | Test Result |
|---|---|---|---|
| styrene content | Internal Method | 0.025 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.