PA12 L1670

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO 11831.01 g/cm
Shrinkage rateASTM D294-40.9-1.1 %
Water absorption rateISO 620.7 %
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusISO 527-21400 Mpa
tensile strength ISO 527-246 Mpa
Tensile strainISO 527-26 %
Tensile strainISO 527-250 %
Charpy Notched Impact StrengthISO 179/1eA4 KJ/m
Electrical performanceTest ConditionTest MethodTest Result
Volume resistivityIEC 600931E+15 Ohm.cm
Dielectric lossIEC 602500.028
Thermal performanceTest ConditionTest MethodTest Result
melting temperatureISO 3146178
Heat distortion temperatureISO 75-2120
Heat distortion temperatureISO 75-250
vicatISO 306/A170
UL flame retardant ratingUL94HB
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.