PA66 SCHULAMID® 66MV HIK 1416

39

Technical Data Sheet

Mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthASTMD63896.0 Mpa
Flexural modulusASTMD7903100 Mpa
Thermal performanceTest ConditionTest MethodTest Result
ASTMD648225 °C
ASTMD64868.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.