TPU Nanguang TPU S-75AX

0
  • Usages:
    General
    industrial applications

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.16到1.20 g/cm³
densityASTMD7921.16到1.20 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore AASTMD224073到77
Shore AASTMD224073到77
Mechanical propertiesTest ConditionTest MethodTest Result
Wear amount30.0 mg
Wear amount30.0 mg
elastomerTest ConditionTest MethodTest Result
tear strengthSplitASTMD47054 kN/m
Tensile stressASTMD4123.43 MPa
Tensile stressASTMD41217.7 MPa
tensile strengthASTMD41229.4 MPa
elongationBreakASTMD412600 %
tear strengthSplitASTMD47054 kN/m
elongationBreakASTMD412600 %
Tensile stressASTMD4123.43 MPa
Tensile stressASTMD41217.7 MPa
tensile strengthASTMD41229.4 MPa
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.