ASA+PA Terblend® S NM-31

0
  • Properties:
    Thermal performance

Technical Data Sheet

Test ConditionTest MethodTest Result
Linear coefficient of thermal expansionISO 11359-21E-04 cm/cm/°C
Surface ResistivityIEC 600931E+14 ohms
Volume resistivityIEC 60093>1.0E+15 ohms·cm
relative permittivityIEC 602502.90
Dissipation FactorIEC 602500.018
densityISO 11831.07 g/cm³
Melt volume flow rateISO 113360.0 cm³/10min
Shrinkage rateISO 294-40.80 %
Water absorption rateISO 621.5 %
Tensile modulusISO 527-22100 MPa
tensile strength ISO 527-250.0 MPa
Tensile strainISO 527-23.3 %
Flexural modulusISO 1782000 MPa
bending strengthISO 17865.0 MPa
elongationBreak25 %
Charpy Notched Impact StrengthISO 1799.0 kJ/m²
Charpy Notched Impact StrengthISO 17970 kJ/m²
Impact strength of cantilever beam gapISO 180/A8.0 kJ/m²
Impact strength of cantilever beam gapISO 180/A65 kJ/m²
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.