physical property Test ConditionTest MethodTest Result
density内部方法0.900to0.940 g/cm³
melt mass-flow rateISO 11335.0to9.0 g/10min
density内部方法0.900to0.940 g/cm³
melt mass-flow rateISO 11335.0to9.0 g/10min
hardnessTest ConditionTest MethodTest Result
Shore hardnessISO 868>50
Shore hardnessISO 868>50
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength YieldISO 527-2>16.0 MPa
tensile strength BreakISO 527-2>12.0 MPa
Tensile strainBreakISO 527-2>50 %
Flexural modulusISO 178700 MPa
tensile strength YieldISO 527-2>16.0 MPa
tensile strength BreakISO 527-2>12.0 MPa
Tensile strainBreakISO 527-2>50 %
Flexural modulusISO 178700 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapISO 180>15 kJ/m²
Impact strength of cantilever beam gapISO 180>15 kJ/m²
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.