TPU ESTANE® 2103-85AE NAT

38

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
melt mass-flow rateASTM D123824 g/10min
Shrinkage rateASTM D9550.0-0.60 %
Shrinkage rateASTM D9550.50-0.70 %
hardnessTest ConditionTest MethodTest Result
Shore hardnessASTM D224088
Shore hardnessASTM D224048
Mechanical propertiesTest ConditionTest MethodTest Result
Taber abraserASTM D10445.00 mg
elastomerTest ConditionTest MethodTest Result
tear strengthASTM D62482.3 kN/m
compression setASTM D395B25 %
compression setASTM D395B80 %
tensile strength ASTM D4125.50 Mpa
tensile strength ASTM D4126.90 Mpa
tensile strength ASTM D41212.1 Mpa
tensile strength ASTM D41232.0 Mpa
elongationASTM D412560 %
Thermal performanceTest ConditionTest MethodTest Result
Glass Transition TemperatureDSC-38.0 °C
vicatASTM D1525267.2 °C
Linear coefficient of thermal expansionASTM D6961.7E-04 cm/cm/°C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.