Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
VOCContent | 0.30 % | ||
0.700到1.40 mm | |||
density | 0.0296 g/cm³ | ||
VOCContent | 9.2 % |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
burning rate | FMVSS302 | 73 mm/min |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
bending strength | ASTMC203 | 0.332 MPa | |
compressive strength | ASTMD1621 | 0.171 MPa | |
ASTMD1621 | 0.187 MPa | ||
ASTMD1621 | 0.225 MPa |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | Break | ASTMD412 | 0.498 MPa |
elongation | Break | ASTMD412 | 12 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Contact Us
Get App