physical property | Test Condition | Test Method | Test Result |
---|
density | | | 1.56 g/cm³ |
Shrinkage Cured | | | 0.15 % |
Cured Properties | Test Condition | Test Method | Test Result |
---|
Supporting hardness | | | 70到78 |
tensile strength | | ASTMD412 | 4.48 MPa |
elongation | Break | ASTMD412 | 70 % |
tear strength | | ASTMD624 | 3.50 kN/m |
arc resistance | | | 125 sec |
electric strength | | | 23 kV/mm |
| | | 3.70 |
Volume resistivity | | | 1E+13 ohms·cm |
Dissipation Factor | | | 0.030 |
Coverage-Cured | | | 0.643 cm³/g |
Supporting hardness | | | 64到72 |
thermosetting | Test Condition | Test Method | Test Result |
---|
| Resin | | 按容量计算的混合比:100按重量计算的混合比:10 |
| Hardener | | 按容量计算的混合比:16按重量计算的混合比:1.0 |
| Shelf Life | | 26 wk |
| | | 15000到25000 cP |
Uncured Properties | Test Condition | Test Method | Test Result |
---|
colour | | | Beige |
| | | 25000到35000 Pa·s |
Curing Time | | | 16到18 hr |
STORAGE STABILITY | | | 60到120 min |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | | 1E-03 cm/cm/°C |
thermal conductivity | | | 0.29 W/m/K |
ServiceTemperature-Cured | | | -51到218 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.