plas
Log In

TPV NOVALAST® 8001 NOVA US

0

Technical Data Sheet

elastomerTest ConditionTest MethodTest Result
tensile strengthBreakASTM D41211.4 MPa
elongationBreakASTM D412590 %
tear strengthASTM D62442.4 kN/m
Permanent compression deformation25°C,22hrASTM D39530 %
Permanent compression deformation70°C,22hrASTM D39544 %
Permanent compression deformation100°C,22hrASTM D39555 %
thermal performanceTest ConditionTest MethodTest Result
Brittle temperatureASTM D746-45.6 °C
Physical propertiesTest ConditionTest MethodTest Result
densityASTM D7920.963 g/cm³
Shrinkage rateMD:3.18mmASTM D9551.5to2.0 %
hardnessTest ConditionTest MethodTest Result
Shore hardnessShoreA,15SecASTM D224080
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.