PA612 VESTAMID® D DX9321

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO 11831.19 g/cm³
Shrinkage rateISO 294-40.90 %
Shrinkage rateISO 294-40.70 %
Water absorption rateISO 622.0 %
Water absorption rateISO 620.80 %
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94HB
Supplementary InformationTest ConditionTest MethodTest Result
ISO ShortcutISO 1874PA612-HI.MH.14-050.GF20
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength BreakISO 527-2/1A115 MPa
Tensile strainYieldISO 527-2/1A-- %
Tensile strainBreakISO 527-2/1A5.0 %
Tensile modulusISO 527-2/1A5700 MPa
tensile strength YieldISO 527-2/1A-- MPa
Impact resistanceTest ConditionTest MethodTest Result
Charpy Notched Impact StrengthISO 179/1eA11 kJ/m²
Charpy Notched Impact StrengthISO 179/1eA18 kJ/m²
Impact strength of simply supported beam without notchISO 179/1eU110 kJ/m²
Impact strength of simply supported beam without notchISO 179/1eU93 kJ/m²
Electrical performanceTest ConditionTest MethodTest Result
relative permittivityIEC 602503.10
Dissipation FactorIEC 602500.050
Dissipation FactorIEC 602500.047
Compared to the Leakage Tracking Index (CTI)IEC 60112PLC 0
Compared to the Leakage Tracking Index (CTI)IEC 60112PLC 0
Volume resistivityIEC 600931E+14 ohms·cm
relative permittivityIEC 602504.40
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureISO 75-2/B208 °C
Heat distortion temperatureISO 75-2/A189 °C
vicatISO 306/B207 °C
melting temperatureISO 11357-3215 °C
Linear coefficient of thermal expansionISO 11359-27E-05 cm/cm/°C
Linear coefficient of thermal expansionISO 11359-25E-05 cm/cm/°C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.