Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.40 g/cm³ |
Water absorption rate | | ASTMD570 | 0.25 % |
Water absorption rate | Saturation | ASTMD570 | 0.90 % |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | M-Scale | ASTMD785 | 90 |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
bending strength | | ASTMD790 | 82.7 MPa |
compressive strength | | ASTMD695 | 103 MPa |
| | | 0.21 |
Flexural modulus | | ASTMD790 | 2520 MPa |
Tensile modulus | | ASTMD638 | 2760 MPa |
tensile strength | | ASTMD638 | 62.1到70.3 MPa |
elongation | Break | ASTMD638 | 30到60 % |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 53 J/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Volume resistivity | | ASTMD257 | 1E+15 ohms·cm |
dielectric strength | | ASTMD149 | 20 kV/mm |
dielectric constant | | ASTMD150 | 3.80 |
dielectric constant | | ASTMD150 | 3.80 |
Dissipation Factor | | ASTMD150 | 3E-03 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD696 | 9.7E-05 cm/cm/°C |
| | ASTMD648 | 104 °C |
Continuous use temperature | | 内部方法 | 85.0 °C |
| | ASTMD3418 | 168 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.