PPS A610MG1 TORAY JAPAN
146
Form:Granules | Grade:Injection grade
Properties:
Low liquidity
Typical Applications:
Automotive Applicationssporting goods
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Automotive Applications | sporting goods |
| Properties: | Low liquidity |
Certificates

Technical Data Sheet
| other | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| characteristic | 流动性.低光泽 | |||
| Color | 黑色 | |||
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
| Impact strength of simply supported beam without notch | 23°C | ISO 179 | 22 | kJ/m² |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 0.73mm | UL 94 | V-0 | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Elongation at Break | ASTM D638/ISO 527 | 1 | % | |
| tensile strength | ASTM D638/ISO 527 | 95 | kg/cm²(MPa)[Lb/in²] | |
| Rockwell hardness | ASTM D785 | 123 | ||
| Bending modulus | ASTM D790/ISO 178 | 20 | kg/cm²(MPa)[Lb/in²] | |
| Charpy Notched Impact Strength | ASTM D256/ISO 179 | 22 | kg·cm/cm(J/M)ft·lb/in | |
| ASTM D256/ISO 179 | 9 | kg·cm/cm(J/M)ft·lb/in | ||
| Taber abraser | 1000Cycles | ISO 9352 | 70.0 | mg |
| Friction coefficient | 0.30 | |||
| shear strength | 23°C | JISK7214 | 60.0 | Mpa |
| bending strength | 23°C | ISO 178 | 245 | Mpa |
| Bending modulus | 23°C | ISO 178 | 20000 | Mpa |
| Tensile strain | Break,23°C | ISO 527-2 | 1.0 | % |
| tensile strength | Yield,23°C | ISO 527-2 | 155 | Mpa |
| bending strength | ASTM D790/ISO 178 | 245 | kg/cm²(MPa)[Lb/in²] | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 2.7E-05 | cm/cm/°C |
| MD | ISO 11359-2 | 1.8E-05 | cm/cm/°C | |
| Melting temperature | ISO 11357-3 | 278 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 260 | °C |
| Combustibility (rate) | UL 94 | V-0 | ||
| Hot deformation temperature | HDT | ASTM D648/ISO 75 | >260 | ℃(℉) |
| Melting temperature | 278 | ℃(℉) | ||
| Linear coefficient of thermal expansion | ASTM D696/ISO 11359 | 1.8 | mm/mm.℃ | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | 23°C,24hr | ISO 62 | 0.020 | % |
| Shrinkage rate | MD:3.00mm4 | Internal Method | 0.20 | % |
| TD:3.00mm2 | Internal Method | 0.60 | % | |
| density | ASTM D792/ISO 1183 | 1.96 | ||
| Shrinkage rate | ASTM D955 | 0.2 | % | |
| Water absorption rate | ASTM D570/ISO 62 | 0.02 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dissipation factor | 23°C,1MHz | IEC 60250 | 2E-03 | |
| Dielectric constant | 23°C,1MHz | IEC 60250 | 4.90 | |
| Dielectric strength | IEC 60243-1 | 22 | KV/mm | |
| Volume resistivity | IEC 60093 | 1E+16 | ohms·cm | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Scale | ISO 2039-2 | 123 | |
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| BarFlowLength | 320°C,1.00mm | Internal Method | 110 | mm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.