Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|
Thermosetting mixed viscosity | | ASTMD2393 | 1500 cP |
stripping time | | | 30到45 min |
| Hardener | | 按重量计算的混合比:1.0,按容量计算的混合比:1.0 |
| | | 5.0-6.0 min |
| Resin | | 按重量计算的混合比:1.0,按容量计算的混合比:1.0 |
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.66 g/cm³ |
Shrinkage rate | | ASTMD955 | 0.080 % |
hardness | Test Condition | Test Method | Test Result |
---|
| | ASTMD2240 | 85 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | Break | ASTMD638 | 44.1 MPa |
compressive strength | | ASTMD695 | 62.7 MPa |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 80.6 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.