| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | -40°C | ISO 180/1A | 8.0 | kJ/m² |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 180 | kJ/m² |
| -30°C | ISO 179/1eU | 160 | kJ/m² | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 8.0 | kJ/m² |
| -30°C | ISO 179/1eA | 7.0 | kJ/m² | |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 8.0 | kJ/m² |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Atomization | G-value(condensate) | ISO 6452 | 3.5E-04 | g |
| F-value(refraction) | ISO 6452 | 90 | % | |
| FMVSS flammability | FMVSS302 | B | ||
| UL flame retardant rating | 1.5mm | IEC 60695-11-10,-20 | HB | |
| 0.8mm | IEC 60695-11-10,-20 | HB | ||
| 1.5mm | UL 94 | HB | ||
| 0.8mm | UL 94 | HB | ||
| Burning rate | 1.00mm | ISO 3795 | 24 | mm/min |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Poisson's ratio | ISO 527 | 0.35 | ||
| Bending modulus | ISO 178 | 3000 | Mpa | |
| Tensile modulus | ISO 527-2 | 3100 | Mpa | |
| tensile strength | Yield | ISO 527-2 | 71.0 | Mpa |
| Tensile strain | Yield | ISO 527-2 | 14 | % |
| Nominal tensile fracture strain | ISO 527-2 | 25 | % | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | TD:AnnealingTime-Optional | ISO 11359-2 | 30.0 | min/mm |
| TD:AnnealingTemperature | ISO 11359-2 | 160 | °C | |
| TD:-40to23°C | ISO 11359-2 | 9E-05 | cm/cm/°C | |
| TD:-- | ISO 11359-2 | 1E-04 | cm/cm/°C | |
| MD:-40to23°C | ISO 11359-2 | 9E-05 | cm/cm/°C | |
| MD:-- | ISO 11359-2 | 1E-04 | cm/cm/°C | |
| Melting temperature | ISO 11357-3 | 178 | °C | |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 162 | °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 96.0 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ISO 1183 | 1.42 | g/cm³ | |
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 15 | g/10min |
| Shrinkage rate | TD | ISO 294-4 | 1.8 | % |
| MD | ISO 294-4 | 2.0 | % | |
| Water absorption rate | Saturation,23°C,2.00mm | ISO 62 | 1.3 | % |
| Equilibrium,23°C,2.00mm,50%RH | ISO 62 | 0.40 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Compared to the anti leakage trace index | IEC 60112 | PLC 0 | ||
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| EmissionofOrganicCompounds | VDA277 | 3.10 | µgC/g | |
| Emission | VDA275 | <8.00 | mg/kg |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.