ASA XC-220-NC KUMHO KOREA
51
Form:Granules | Grade:Injection grade
Properties:
High impact resistanceHigh impact
Typical Applications:
Electronic fieldElectrical fieldLaptop caseLaptop caseemailElectronic and electrical components
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Electronic field | Electrical field | Laptop case | Laptop case | email | Electronic and electrical components |
| Properties: | High impact resistance | High impact |
Certificates
No Data...
Technical Data Sheet
| Basic Performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| melt mass-flow rate | 220℃/10kg | ASTM-D1238 | 12 | g/10min |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | ASTM-D638 | 47 | Mpa | |
| elongation | ASTM-D638 | 30 | % | |
| bending strength | ASTM-D790 | 60 | Mpa | |
| Bending modulus | ASTM-D790 | 1800 | Mpa | |
| Impact strength of cantilever beam gap | 3.2mm,Notched | ASTM-D256 | 220 | J/m |
| Rockwell hardness | ASTM-D785 | 100 | R-Scale | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.82Mpa | ASTM-D648 | 85 | °C |
| Vicat softening temperature | ASTM-D1525 | 96 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | ASTM-D792 | 1.08 | g/10min | |
| Shrinkage rate | ASTM-D955 | 0.4-0.7 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.