PEEK Pyramid™ PEEK KD2000 CAM Tube Polymics, Ltd.
0
Technical Data Sheet
| flammability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| UL flame retardant rating | UL 94 | V-0 | |
| Extreme Oxygen Index | ASTM D2863 | 38 % |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| bending strength | ASTM D790 | 137 MPa | |
| Tensile modulus | ASTM D638 | 3400 MPa | |
| tensile strength | ASTM D638 | 105 MPa | |
| elongation | Break | ASTM D638 | >30 % |
| Bending modulus | 143°C | ASTM D790 | 3400 MPa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 150 °C |
| Melting temperature | DSC | 340 °C | |
| Linear coefficient of thermal expansion | MD | ASTM D696 | 4.7E-06 cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | ASTM D792 | 1.30 g/cm³ | |
| Water absorption rate | 23°C,24hr | ASTM D570 | 0.20 % |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Surface resistivity | ASTM D257 | 1E+14 ohms | |
| Volume resistivity | ASTM D257 | 1E+14 ohms·cm | |
| Dielectric strength | ASTM D149 | 21 kV/mm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.