PUR-Ether/MDI Andur M-10 (1,4BD)

0

Technical Data Sheet

thermosettingTest ConditionTest MethodTest Result
STORAGE STABILITY3.0 min
stripping time30 min
hardnessTest ConditionTest MethodTest Result
ASTMD224060
elastomerTest ConditionTest MethodTest Result
Tensile stressASTMD41219.2 MPa
Tensile stressASTMD41223.8 MPa
tensile strengthYieldASTMD41235.9 MPa
elongationBreakASTMD412440 %
compression setASTMD39537 %
Basho elasticityASTMD263248 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.