PS Diamond HIPS HI-860

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.05 g/cm³
melt mass-flow rateASTMD12385.0 g/10min
Water absorption rate<0.10 %
Water absorption rateEquilibrium<0.10 %
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthYieldASTMD63816.7 MPa
tensile strengthBreakASTMD63816.7 MPa
elongationBreakASTMD63855 %
bending strengthASTMD79029.4 MPa
Impact resistanceTest ConditionTest MethodTest Result
Suspended wall beam without notch impact strengthASTMD256150 J/m
Falling hammer impactASTMD25612.4 J
Thermal performanceTest ConditionTest MethodTest Result
ASTMD64890.0 °C
vicatASTMD1525100 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.