Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|
| | | 按重量计算的混合比:100按容量计算的混合比:3.0 |
| | | 按重量计算的混合比:43按容量计算的混合比:1.0 |
| | | 35到45 min |
Thermosetting mixed viscosity | | ASTMD2393 | 150到250 cP |
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.01到1.06 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
| | ASTMD2240 | 77到83 |
Electrical performance | Test Condition | Test Method | Test Result |
---|
dielectric strength | | ASTMD149 | 16到17 kV/mm |
dielectric constant | | ASTMD2520 | 3.19到3.52 |
Dissipation Factor | | ASTMD150 | 0.042到0.046 |
Volume resistivity | | ASTMD257 | 1.1E+13到1.2E+13 ohms·cm |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Glass Transition Temperature | | ASTME1356 | -23.0到-21.0 °C |
| | ASTMD696 | 1.9E-4到2.1E-4 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.