Test Condition | Test Method | Test Result | |
---|---|---|---|
无缺口伊佐德冲击强度 | ISO180 | 45 kJ/m² | |
热变形温度 | 1.8MPa,未退火 | ASTMD648A | 190 °C |
维卡软化温度 | ASTMD15252 | 175 °C | |
RTI Elec | UL746 | 110 °C | |
RTI Imp | UL746 | 110 °C | |
RTI | UL746 | 110 °C | |
抗张强度 | Yield | ASTMD638 | 115 MPa |
伸长率 | Break | ASTMD638 | 2.5 % |
悬壁梁缺口冲击强度 | ISO180/A | 12 kJ/m² | |
密度 | ASTMD792 | 1.23 g/cm³ | |
收缩率 | MD | ASTMD955 | 0.40 % |
TD | ASTMD955 | 0.60 % | |
拉伸模量 | ASTMD638 | 8500 MPa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.