Technical Data Sheet

Cured PropertiesTest ConditionTest MethodTest Result
elongationBreakASTM D638250 %
tensile strengthASTM D63811.7 MPa
Shore hardnessShoreAASTM D224065to75
tear strengthASTM D62431.5 kN/m
Uncured PropertiesTest ConditionTest MethodTest Result
viscosity固化时间(25°C)1.7E+02 hr
viscosity25°C41.5 Pa·s
viscosity25°C30.98 Pa·s
viscosity25°C20.10 Pa·s
viscosityGelTime7.0to13 min
thermosettingTest ConditionTest MethodTest Result
Thermosetting componentsDemold Time360to600 min
Thermosetting componentsHardener按重量计算的混合比:100按容量计算的混合比:100
Thermosetting componentsResin按重量计算的混合比:34按容量计算的混合比:29
Physical propertiesTest ConditionTest MethodTest Result
densityCured1.12 g/cm³
densityHardener1.04 g/cm³
Shrinkage rateMDASTM D25660.10to0.50 %
density基体Resin1.20 g/cm³
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.