TPE 2160
0
- Properties:Injection molding reference process: temperature at the rear of the barrel140-160 ℃holding pressure30-120MPatemperature at the middle of the barrel150-170 ℃mold temperature20-50 ℃temperature at the front of the barrel160-180 ℃holding time15-75S nozzle temperature170-190 ℃screw speed20-100rmininjection pressure40-150MPainjection speedmedium fast back pressure
Technical Data Sheet
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
relative density | 1.16 g/cm |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | 9.5 MPa | ||
Elongation | 440 % | ||
stretching strength | 3.0 MPa | ||
tear strength | 29.0 kN/m | ||
Shore hardness | 60 A |
Other performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile strength retention rate | 113 % | ||
Constant tensile strength retention rate | 123 % | ||
Volume change of fuel B | -15 % | ||
permanent set | 35 % | ||
Retention rate of elongation at break | 95 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.