Share
Add to compare

Epoxy M10-D Epoxy Technology Inc.

Product Description
Certificates(0)
Datasheet

Product Description

Certificates

No Data...

Technical Data Sheet

Cured PropertiesTest ConditionTest MethodTest ResultTest Unit
Shore hardnessShoreD72
LapShearStrength23°C4.00MPa
Dissipation factor1kHz0.11
Volume resistivity23°C>5.0E+11ohms·cm
Relative permittivity1kHz4.32
Uncured PropertiesTest ConditionTest MethodTest ResultTest Unit
Curing timePot Life720000min
Curing time150°C1.0hr
Curing time75°C60.50hr
viscosity23°C3.0to6.0Pa·s
density1.35g/cm³
ColorTan
thermosettingTest ConditionTest MethodTest ResultTest Unit
drying time>1.0day
shelf-life52wk
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Linear coefficient of thermal expansionMD:导热系数0.42W/m/K
Linear coefficient of thermal expansionMD:--31.3E-04cm/cm/°C
Linear coefficient of thermal expansionMD:--23.5E-05cm/cm/°C
Glass transition temperature80.0°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
Particle size distribution<20.0µm
Supplementary InformationTest ConditionTest MethodTest ResultTest Unit
weight loss on heating250°C2.8%
weight loss on heating200°C1.3%
operate temperatureThixotropicIndex9.20
operate temperatureStorageModulus(23°C)3.98GPa
operate temperatureIntermittent-55-300°C
operate temperatureContinuous-55-200°C
Shear Strength23°C23.4MPa
DegradationTemperature370°C
weight loss on heating300°C5.8%
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.