TPV Alloy Elastoprene 40D-4000 KMI Group, Inc.

0

Technical Data Sheet

elastomerTest ConditionTest MethodTest Result
tensile strength100%Strain,23°CASTM D4129.00 MPa
tensile strengthYield,23°CASTM D41218.0 MPa
elongationBreak,23°CASTM D4121100 %
tear strength23°CASTM D62482.0 kN/m
Permanent compression deformation70°C,22hrASTM D39542 %
Permanent compression deformation125°C,70hrASTM D39573 %
thermal performanceTest ConditionTest MethodTest Result
Melting temperature159 °C
Brittle temperatureASTM D746-70.0 °C
Physical propertiesTest ConditionTest MethodTest Result
densityASTM D7920.960 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardnessShoreD,5SecASTM D224040
Shore hardnessShoreD,15SecASTM D224038
Supplementary InformationTest ConditionTest MethodTest Result
ozone resistanceASTM D1149Excellent
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.