PC/ABS LS-1159 K21441 Samsung Cheil South Korea
106
Form:Granules | Grade:Injection grade
Properties:
Glass fiber reinforcedFlame retardantFiller: Glass fiber reinf
Typical Applications:
Tool handleTV
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Tool handle | TV |
| Properties: | Glass fiber reinforced | Flame retardant | Filler: Glass fiber reinf |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 6.0 | kJ/m² |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 6.0 | kJ/m² |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 3.0mm | UL 94 | V-0 | |
| 2.5mm | UL 94 | V-0 | ||
| 2.0mm | UL 94 | V-0 | ||
| 1.5mm | UL 94 | V-1 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Bending modulus | ISO 178 | 5000 | Mpa | |
| ASTM D790 | 4700 | Mpa | ||
| Tensile strain | Break | ISO 527-2/5 | 3.3 | % |
| elongation | Break | ASTM D638 | 3.3 | % |
| tensile strength | Break | ISO 527-2/5 | 90.0 | Mpa |
| Break | ASTM D638 | 88.0 | Mpa | |
| Yield | ISO 527-2/5 | 80.0 | Mpa | |
| Yield | ASTM D638 | 78.0 | Mpa | |
| Tensile modulus | ISO 527-2/5 | 4400 | Mpa | |
| ASTM D638 | 4300 | Mpa | ||
| bending strength | ISO 178 | 110 | Mpa | |
| ASTM D790 | 120 | Mpa | ||
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8MPa,Unannealed,6.40mm | ASTM D648 | 91.0 | °C |
| 0.45MPa,Unannealed,6.40mm | ASTM D648 | 96.0 | °C | |
| Vicat softening temperature | ISO 306/B50 | 97.0 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed,4.00mm | ISO 75-2/A | 91.0 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | 250°C/2.16kg | ASTM D1238 | 14 | g/10min |
| 250°C/2.16kg | ISO 1133 | 14 | g/10min | |
| Shrinkage rate | MD:3.20mm | ASTM D955 | 0.10 | % |
| TD:3.20mm | ASTM D955 | 0.10 | % | |
| TD:3.20mm | ISO 2577 | 0.10 | % | |
| MD:3.20mm | ISO 2577 | 0.10 | % | |
| ash content | -- | ISO 3451 | 15 | % |
| -- | ASTM D5630 | 15 | % | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Scale | ISO 2039-2 | 120 | |
| R-Scale | ASTM D785 | 120 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.