SEBS G P.G401.A70.N
0
- Properties:BlockCopolymerAdhesiveGood ColorabilitySoft
- Usages:Application in medical and nursing fields
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D792 | 0.890 g/cm³ | |
Shrinkage rate | ASTM D955 | 2.4 % | |
1.2 | |||
density | ASTMD792 | 0.890 g/cm³ | |
Shrinkage rate | ASTMD955 | 2.4 % | |
ASTMD955 | 1.2 % |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore A | ASTMD2240 | 70 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
OzoneResistance-Stress | ASTMD518 | NoCracks | |
Ozone Resistance - Stressed | ASTM D518 | No Cracks |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
hardness | ASTM D2240 | 70 | |
Tensile stress | ASTM D412 | 2.60 MPa | |
4.10 | |||
tensile strength | Break | ASTM D412 | 10.0 MPa |
elongation | Break | ASTM D412 | 950 % |
tear strength | ASTM D624 | 45.0 kN/m | |
compression set | ASTM D395 | 19 % | |
43 | |||
68 |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | Break | ASTMD412 | 10.0 MPa |
elongation | Break | ASTMD412 | 950 % |
tear strength | ASTMD624 | 45.0 kN/m | |
compression set | ASTMD395 | 19 % | |
ASTMD395 | 43 % | ||
ASTMD395 | 68 % | ||
Tensile stress | ASTMD412 | 2.60 MPa | |
ASTMD412 | 4.10 MPa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.