Epoxy GE116 Epoxy Technology Inc.
Product Description
Certificates(0)
Datasheet
Product Description
Certificates
No Data...
Technical Data Sheet
| Cured Properties | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Relative permittivity | 1kHz | 3.48 | ||
| LapShearStrength | 23°C | 10.8 | MPa | |
| Shore hardness | ShoreD | 80 | ||
| Dissipation factor | 1kHz | 7E-03 | ||
| Volume resistivity | 23°C | >7.0E+13 | ohms·cm | |
| Uncured Properties | Test Condition | Test Method | Test Result | Test Unit |
| storage stability | 40000 | min | ||
| Curing time | 150°C | 1.0 | hr | |
| viscosity | 23°C | 200to300 | Pa·s | |
| density | 1.15 | g/cm³ | ||
| Color | Red | |||
| thermosetting | Test Condition | Test Method | Test Result | Test Unit |
| shelf-life | -40°C | 52 | wk | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | MD:--4 | 2.2E-04 | cm/cm/°C | |
| MD:--3 | 4.1E-05 | cm/cm/°C | ||
| Glass transition temperature | >65.0 | °C | ||
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Particle size distribution | <20.0 | µm | ||
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| weight loss on heating | 250°C | 1.1 | % | |
| 200°C | 0.27 | % | ||
| operate temperature | StorageModulus(23°C) | 3.02 | GPa | |
| Intermittent | -55-275 | °C | ||
| Continuous | -55-175 | °C | ||
| Shear Strength | 23°C | 11.7 | MPa | |
| DegradationTemperature | 344 | °C | ||
| weight loss on heating | 300°C | 3.0 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.