Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ISO1183 | 0.900 g/cm³ |
melt mass-flow rate | | ASTMD1238 | 25 g/10min |
optical performance | Test Condition | Test Method | Test Result |
---|
Haze ratio | | ASTMD1003 | 6.0 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ISO527-2/1 | 1150 MPa |
Tensile stress | Yield | ISO527-2/50 | 29.0 MPa |
Tensile strain | Yield | ISO527-2/50 | 11 % |
Tensile strain | Break | ISO527-2/50 | >50 % |
Flexural modulus | | ISO178 | 1200 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Charpy Notched Impact Strength | | ISO179/1e | 3.0 kJ/m² |
Charpy Notched Impact Strength | | ISO179/1e | 6.0 kJ/m² |
Impact strength of simply supported beam without notch | | ISO179/1eU | 70 kJ/m² |
Impact strength of simply supported beam without notch | | ISO179/1eU | 200 kJ/m² |
Impact strength of cantilever beam gap | | ISO180 | 5.4 kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result |
---|
vicat | | ISO306/A50 | 130 °C |
| | ISO75-2/B | 76.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.