TPE 2175
0
- Properties:Injection molding reference process: temperature at the rear of the barrel140-160 ℃holding pressure30-120MPatemperature at the middle of the barrel150-170 ℃mold temperature20-50 ℃temperature at the front of the barrel160-180 ℃holding time15-75S nozzle temperature170-190 ℃screw speed20-100rmininjection pressure40-150MPainjection speed?
Technical Data Sheet
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
relative density | 1.23 g/cm |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Elongation | 400 % | ||
Shore hardness | 75 A | ||
tensile strength | 13.0 MPa | ||
stretching strength | 5.0 MPa | ||
tear strength | 45.0 kN/m |
Other performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Retention rate of elongation at break | 96 % | ||
Volume change of fuel B | -10 % | ||
Tensile strength retention rate | 110 % | ||
permanent set | 41 % | ||
Constant tensile strength retention rate | 121 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.