Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.27 g/cm³ |
Shrinkage rate | | ASTMD955 | 0.20to0.50 % |
Water absorption rate | | ASTMD570 | 0.13 % |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | | ASTMD785 | 106 |
optical performance | Test Condition | Test Method | Test Result |
---|
transmissivity | | ASTMD1003 | 91.0 % |
transmissivity | | ASTMD1003 | 88.0 % |
Haze ratio | | ASTMD1003 | 0.30 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
bending strength | | ASTMD790 | 70.0 MPa |
tensile strength | | ASTMD638 | 50.0 MPa |
tensile strength | | ASTMD638 | 28.0 MPa |
elongation | | ASTMD638 | 4.3 % |
elongation | | ASTMD638 | 110 % |
Flexural modulus | | ASTMD790 | 2100 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 37 J/m |
Impact strength of cantilever beam gap | | ASTMD256 | 100 J/m |
Impact strength of cantilever beam gap | | ASTMD4218 | NoBreak |
Impact strength of cantilever beam gap | | ASTMD4218 | NoBreak |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Heat distortion temperature | | ASTMD648 | 63.0 °C |
Heat distortion temperature | | ASTMD648 | 70.0 °C |
vicat | | ASTMD1525 | 85.0 °C |
specific heat | | ASTMD2766 | 1300 J/kg/°C |
specific heat | | ASTMD2766 | 2010 J/kg/°C |
specific heat | | ASTMD2766 | 0.19 W/m/K |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.