Epoxy Ablebond 967-3

0

Technical Data Sheet

thermosettingTest ConditionTest MethodTest Result
STORAGE STABILITY2900 min
shelf-life52 wk
shelf-life52 wk
shelf-life26 wk
shelf-life7000 cP
Post curing time6.0 hr
Post curing time0.50 hr
Supplementary InformationTest ConditionTest MethodTest Result
Ionic Chloride<300 ppm
IonicPotassium<30 ppm
IonicSodium<10 ppm
LapShear-Aluminum>1700
MixingRatio-PartA:PartB1:1
ShearStrength-Gold108 N
WaterExtractConductivity80.0 µS/cm
Electrical performanceTest ConditionTest MethodTest Result
Volume resistivity2E+13 ohms·cm
dielectric constant4.30
Dissipation Factor0.025
Thermal performanceTest ConditionTest MethodTest Result
Glass Transition Temperature85.0 °C
thermal conductivity0.70 W/m/K
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.