AS(SAN) KIBISAN PN-108L125
645
- Properties:transparentHigh mobility
- Usages:chipcontainerThin walled products
- Certificates:MSDS
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
melt mass-flow rate | ASTM D-1238 | 5.0 g/10min | |
ISO 1133 | 5 cm3/10min |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
burning rate | 1.5mm HB | ||
elongation at break | ASTM D-638 | 5.0 % | |
50 mm/min | 5 % | ||
bending strength | 2mm/min | 101 Mpa | |
tensile strength | 50 mm/min | 67 Mpa | |
Impact strength of cantilever beam gap | 4mm/23℃ | 3.8 kJ/m² | |
ASTM D-256 | 1.8 kg.cm/cm | ||
Flexural modulus | 2 mm/min | 3.4 GPa | |
Thermal performance | ASTM D-1525 | 106(104) °C | |
Shore hardness | ASTM D-785 | M-83 R scale | |
density | ISO 1183 | 1.07 - | |
Flexural modulus | ASTM D-790 | 35000 kg/cm2 | |
tensile strength | ASTM D-638 | 600 kg/cm2 | |
bending strength | ASTM D-790 | 900 kg/cm2 | |
Shore hardness | ASTM D785 | M-83 M-scale | |
burning rate | UL 94 | HB | |
vicat | 50℃/hr | 105 ℃ | |
Heat distortion temperature | 未退火 | 86 ℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.