Technical Data Sheet
Test Condition | Test Method | Test Result | |
---|---|---|---|
Heat distortion temperature | ISO 75-2/Af | 78.0 °C | |
vicat | ISO 306/A50 | 184 °C | |
ISO 306/B50 | 110 °C | ||
burning rate | ISO 3795 | 30 mm/min | |
UL flame retardant rating | IEC 60695-11-10,-20 | HB | |
density | ISO 1183/A | 1.18 g/cm³ | |
Melt volume flow rate | ISO 1133 | 6.00 cm³/10min | |
Tensile modulus | ISO 527-2/1A/1 | 3100 MPa | |
tensile strength | Yield | ISO 527-2/1A/50 | 51.0 MPa |
Tensile strain | Yield | ISO 527-2/1A/50 | 3.1 % |
Charpy Notched Impact Strength | ISO 179/1eA | 4.0 kJ/m² | |
UL flame retardant rating | IEC 60695-11-10,-20 | HB | |
Burning wire flammability index | IEC 60695-2-12 | 675 °C | |
IEC 60695-2-12 | 675 °C | ||
Hot filament ignition temperature | IEC 60695-2-13 | 700 °C | |
IEC 60695-2-13 | 700 °C | ||
Charpy Notched Impact Strength | ISO 179/1eA | 10 kJ/m² | |
Impact strength of simply supported beam without notch | ISO 179/1eU | 75 kJ/m² | |
ISO 179/1eU | NoBreak | ||
ball-indentation hardness | ISO 2039-1 | 101 MPa | |
Heat distortion temperature | ISO 75-2/Bf | 96.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.