Share
Add to Compare

LLDPE 2517 STYRON US

20

Form:Granules | Grade:Injection grade

Product Description
Certificates(0)
Datasheet

Product Description

Certificates

No Data...

Technical Data Sheet

impact performanceTest ConditionTest MethodTest ResultTest Unit
Impact strength of cantilever beam gapASTM D1822399kJ/m²
Basic PerformanceTest ConditionTest MethodTest ResultTest Unit
densityASTM D-7920.917g/m
melt mass-flow rate190℃/2.16kgASTM D-123825g/10min
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
Elongation at BreakASTM D-638600%
Bending modulus2% SecantASTM D-790B234Mpa
Impact strength of cantilever beam gapASTM D-1822399KJ/m
Shore hardnessShore DASTM D-224045
Environmental stress cracking resistance50℃,100% Igepal,F50ASTM D-16934hr
tensile strengthYieldASTM D-6389.65Mpa
tensile strengthBreakASTM D-6388.96Mpa
elongation at yieldASTM D-6383%
tensile strengthYieldASTM D6389.65Mpa
tensile strengthBreakASTM D6388.96Mpa
elongationYieldASTM D6383.0%
elongationBreakASTM D638600%
Bending modulus2%SecantASTM D790B234Mpa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Hot deformation temperature0.45MPa,UnannealedASTM D-64839.4°C
Vicat softening temperatureASTM D-152591.7°C
Melting temperatureInternal Method124°C
Crystallization peak temperatureInternal Method103°C
Vicat softening temperatureASTM D152591.7°C
Melting temperatureInternal Method124°C
Crystallization peak temperatureDSCInternal Method103°C
Hot deformation temperature0.45MPa,UnannealedASTM D64839.4°C
Brittle temperatureASTM D746<-76.1°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
melt mass-flow rate190°C/2.16kgASTM D123825g/10min
Environmental stress cracking resistance50°C,100%Igepal,F50ASTM D16934.00hr
hardnessTest ConditionTest MethodTest ResultTest Unit
Shore hardnessShoreDASTM D224045
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.