HIPS PS-350 GPPC TAIWAN

453

Technical Data Sheet

物理性能Test ConditionTest MethodTest Result
密度ASTMD7921.05 g/cm³
熔体质量流动速率200°C/5.0kgASTMD12384.8 g/10min
熔体质量流动速率230°C/3.8kgASTMD123814 g/10min
热性能Test ConditionTest MethodTest Result
热变形温度1.8MPa,未退火,12.7mmASTMD64882.0 °C
可燃性Test ConditionTest MethodTest Result
UL阻燃等级1.6mmUL94HB
UL阻燃等级3.2mmUL94HB
机械性能Test ConditionTest MethodTest Result
抗张强度3.18mmASTMD63828.4 Mpa
弯曲模量3.18mmASTMD7902060 Mpa
弯曲强度3.18mmASTMD79047.1 Mpa
硬度Test ConditionTest MethodTest Result
洛氏硬度L计秤ASTMD78558
冲击性能Test ConditionTest MethodTest Result
悬壁梁缺口冲击强度3.18mmASTMD25698 J/m
悬壁梁缺口冲击强度6.35mmASTMD25683 J/m
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.