PC/PBT 1105-78211 SABIC INNOVATIVE SHANGHAI
168
Form:Granules | Grade:Impact resistant grade
Properties:
Chemical resistanceLow temperature impact re
Typical Applications:
Household daily necessitiesElectrical applicationsAutomotive Applications
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Household daily necessities | Electrical applications | Automotive Applications |
| Properties: | Chemical resistance | Low temperature impact re |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| 23°C | ISO 180/1A | 63 | kJ/m² | |
| -10°C | ASTM D256 | 700 | J/m | |
| -20°C | ASTM D256 | 690 | J/m | |
| -30°C | ASTM D256 | 490 | J/m | |
| -40°C | -40℃ | ASTM D256 | 370 | J/m |
| -30°C | ISO 180/1A | 51 | kJ/m² | |
| -40°C18 | -40℃ | ISO 180/1A | 35 | kJ/m² |
| 23°C | ASTM D256 | 760 | J/m | |
| 0°C | ASTM D256 | 720 | J/m | |
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 48 | kJ/m² |
| 23°C | ISO 179/1eA | 63 | kJ/m² | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| --1 | ASTM D638 | 1990 | Mpa | |
| --2 | ASTM D638 | 2020 | Mpa | |
| crack | ASTM D638 | 110 | % | |
| yield | ISO 527-2/50 | 4.5 | % | |
| ASTM D638 | 4.2 | % | ||
| ASTM D638 | 4.1 | % | ||
| crack | ISO 527-2/50 | 50.5 | Mpa | |
| ASTM D638 | 47.4 | Mpa | ||
| ASTM D638 | 46.0 | Mpa | ||
| yield | ISO 527-2/50 | 52.4 | Mpa | |
| ASTM D638 | 48.8 | Mpa | ||
| ASTM D638 | 45.2 | Mpa | ||
| crack | ASTM D638 | 120 | % | |
| ISO 527-2/50 | 120 | % | ||
| 50.0mm span | ASTM D790 | 1900 | Mpa | |
| --12 | ISO 178 | 2020 | Mpa | |
| --13 | ISO 178 | 78.9 | Mpa | |
| Yield, 50.0mm span | ASTM D790 | 76.1 | Mpa | |
| Fracture, 50.0mm span | ASTM D790 | 74.7 | Mpa | |
| Fracture bending strain | ISO 178 | 7.3 | % | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| 0.45MPa, unannealed, 6.40mm | ASTM D648 | 115 | °C | |
| 0.45MPa, unannealed, 64.0mm span | ISO 75-2/Bf | 109 | °C | |
| 1.8MPa, unannealed, 6.40mm | ASTM D648 | 97.0 | °C | |
| 1.8MPa, unannealed, 64.0mm span of | ISO 75-2/Af | 90.2 | °C | |
| Vicat softening temperature | ASTMD1525 | 123 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Specific volume | ASTM D792 | 1.20 | cm³/g | |
| Shrinkage rate | TD:3.20mm | Internal Method | 0.80-1.0 | % |
| MD:3.20mm | Internal Method | 0.80-1.0 | % | |
| melt mass-flow rate | 250°C/5.0kg | ASTMD1238 | 16 | g/10min |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreD | ISO 868 | 79 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.