LMDPE ICORENE® 3933

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
Environmental stress cracking resistanceASTM D1693A>1000 hr
densityASTM D15050.939 g/cm³
melt mass-flow rateASTM D12383.3 g/10min
Environmental stress cracking resistanceASTM D1693A145 hr
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength YieldASTM D63820.5 MPa
elongationBreakASTM D638>1000 %
Flexural modulusASTM D790760 MPa
agingTest ConditionTest MethodTest Result
Accelerated agingASTMG2611.0 month
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D64860.0 °C
Heat distortion temperatureASTM D64841.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.