Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ISO 1183 | 1.50 g/cm³ |
Shrinkage rate | | 内部方法 | 0.30 % |
Water absorption rate | | ISO 62 | 1.5 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ISO 527-2 | 13000 MPa |
Tensile modulus | | ISO 527-2 | 8800 MPa |
Tensile modulus | | ISO 527-2 | 7800 MPa |
tensile strength | | ISO 527-2 | 220 MPa |
tensile strength | | ISO 527-2 | 145 MPa |
tensile strength | | ISO 527-2 | 125 MPa |
Tensile strain | Break | ISO 527-2 | 2.2 % |
Flexural modulus | | ISO 178 | 10900 MPa |
bending strength | | ISO 178 | 330 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Charpy Notched Impact Strength | | ISO 179 | 30 kJ/m² |
Impact strength of simply supported beam without notch | | ISO 179 | 70 kJ/m² |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Compared to the Leakage Tracking Index (CTI) | | IEC 60112 | PLC 1 |
dielectric strength | | IEC 60243-1 | 35 kV/mm |
Surface Resistivity | | ASTM D257 | 1E+12 ohms |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Heat distortion temperature | | ISO 75-2/A | 237 °C |
Linear coefficient of thermal expansion | | ISO 7991 | 2.3E-05 cm/cm/°C |
thermal conductivity | | ISO 22007 | 0.33 W/m/K |
Heat distortion temperature | | ISO 75-2/B | 245 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.