PBT PB70 GR20 IH MELOS GERMANY
8
- Properties:Low friction coefficientImpact resistanceThermal insulationAging resistanceHigh glossDimensional stabilityFiller: Glass fiber reinf20% filler by weight
- Usages:Electronic fieldElectrical field
Technical Data Sheet
| other | Test Condition | Test Method | Test Result |
|---|---|---|---|
| characteristic | 本色加纤 | ||
| purpose | 电子电工器材 |
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 65 kJ/m² |
| -30°C | ISO 180/1U | 60 kJ/m² |
| flammability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot filament ignition temperature | 2.0mm | IEC 60695-2-13 | 725 °C |
| Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 960 °C |
| UL flame retardant rating | 1.6mm | UL 94 | V-0 |
| 0.75mm | UL 94 | V-2 |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Tensile strain | Break,23°C | ISO 527-2 | 3.0 % |
| tensile strength | Break,23°C | ISO 527-2 | 100 Mpa |
| Tensile modulus | 23°C | ISO 527-2 | 7500 Mpa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 215 °C |
| Melting temperature | ISO 11357-3 | 225to255 °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 175 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| water content | ISO 15512 | <0.080 % | |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.20 % |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Compared to the anti leakage trace index | SolutionA | IEC 60112 | PLC 3 |
| Volume resistivity | IEC 60093 | 1E+16 ohms·cm | |
| Surface resistivity | IEC 60093 | 1E+14 ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.