PCT Infino TK-2046HM

0
  • Properties:
    Fillers
    glass fiber reinforced materials

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
Ash ContentISO345141 %
Ash ContentASTMD563041 %
densityASTMD7921.61 g/cm³
densityISO11831.61 g/cm³
melt mass-flow rateASTMD123820 g/10min
melt mass-flow rateISO113320 g/10min
optical performance Test ConditionTest MethodTest Result
Yellowness IndexASTMD19254.0 YI
Yellowness IndexASTMD19254.0 YI
Mechanical propertiesTest ConditionTest MethodTest Result
elongationBreakASTMD6381.5 %
Tensile strainBreakISO527-2/51.5 %
tensile strengthYieldASTMD63861.0 MPa
Tensile stressYieldISO527-2/5620 MPa
Flexural modulusASTMD7907600 MPa
Flexural modulusISO17877000 MPa
bending strengthASTMD79078.0 MPa
Bending stressISO178800 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD256150 J/m
UnnotchedIzodImpactStrengthISO180/1U16 kJ/m²
Charpy Notched Impact StrengthISO179/1eA2.8 kJ/m²
Impact strength of simply supported beam without notchISO179/1eU13 kJ/m²
Impact strength of cantilever beam gapASTMD25629 J/m
Impact strength of cantilever beam gapASTMD25629 J/m
Impact strength of cantilever beam gapISO180/1A3.0 kJ/m²
Impact strength of cantilever beam gapASTMD256160 J/m
Thermal performanceTest ConditionTest MethodTest Result
ASTMD648250 °C
ISO75-2/A250 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.