SBR, Emulsion SIBUR Synthetic Rubber SBR-1706 Grade D SIBUR RUSSIA
0
Technical Data Sheet
| elastomer | Test Condition | Test Method | Test Result |
|---|---|---|---|
| elongation | Break | ASTM D3185 | >400 % |
| tensile strength | 300%Strain | ASTM D3185 | >9.80 MPa |
| Yield | ASTM D3185 | >21.0 MPa |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Mooney viscosity | ML1+4,100°C | ASTM D1646 | 36to44 MU |
| Combining styrene | Internal Method | 22.0to25.0 % | |
| OilContent-HI-ARorTDAE | Internal Method | 14to17 % | |
| Organic Acid | ASTM D5774 | 5.0to6.4 % | |
| soap content | 有机酸 | ASTM D5774 | <0.25 % |
| Solvent content | Internal Method | 19to25 % | |
| ash content | ASTM D5667 | <0.60 % | |
| Volatile compounds | ASTM D5668 | <0.60 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.