PBT LOXIM 220 12 HB

0
  • Properties:
    Filler
    glass fiber reinforced material
    20%
    filler by weight

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.45 g/cm³
Shrinkage rateASTMD12990.60到0.80 %
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL94HB
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusASTMD6385500 MPa
tensile strengthBreakASTMD63880.0 MPa
elongationBreakASTMD6383.0 %
Flexural modulusASTMD7905500 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD25645 J/m
Thermal performanceTest ConditionTest MethodTest Result
ASTMD648B210到215 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.

Contact Us

Get App

Top