Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ISO1183 | 1.65到1.80 g/cm³ |
Apparent density | | ISO60 | 0.60到0.80 g/cm³ |
Shrinkage rate | | ISO2577 | 0.30到0.50 % |
Water absorption rate | | ISO62 | <0.20 % |
PostShrinkage | | ISO2577 | <0.20 % |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | V-0 |
Burning wire flammability index | | IEC60695-2-12 | 960 °C |
Hot filament ignition temperature | | IEC60695-2-13 | 960 °C |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | Injection | ISO527-2 | 6000到9000 MPa |
Tensile stress | | ISO527-2 | 70.0到90.0 MPa |
Tensile stress | Injection | ISO527-2 | 90.0到110 MPa |
Flexural modulus | Compression Molded | ISO178 | 11000到13000 MPa |
Flexural modulus | Injection | ISO178 | 12000到14000 MPa |
Bending stress | Compression Molded | ISO178 | 110到140 MPa |
Bending stress | Injection | ISO178 | 150到180 MPa |
compression stress | | ISO604 | 250到300 MPa |
Tensile modulus | Compression Molded | ISO527-2 | 6000到9000 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of simply supported beam without notch | Compression Molded | ISO179/1eU | 7.0到10 kJ/m² |
Impact strength of simply supported beam without notch | Injection | ISO179/1eU | 13到17 kJ/m² |
Charpy Notched Impact Strength | Injection | ISO179/1eA | 3.0到5.0 kJ/m² |
Charpy Notched Impact Strength | Compression Molded | ISO179/1eA | 2.0到4.0 kJ/m² |
Electrical performance | Test Condition | Test Method | Test Result |
---|
CTI | | IEC60112 | >225 V |
Surface Resistivity | | IEC60093 | 1.0E+10到1.0E+11 ohms |
Volume resistivity | | IEC60093 | 1.0E+12到1.0E+13 ohms·cm |
dielectric strength | | IEC60243-1 | 20到30 kV/mm |
| | IEC60250 | 6.008.00 |
| | IEC60250 | 4.006.00 |
Dissipation Factor | | IEC60250 | 0.010到0.020 |
Dissipation Factor | | IEC60250 | 0.020到0.030 |
arc resistance | | ASTMD495 | PLC 4 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ISO11359-2 | 1.4E-5到1.6E-5 cm/cm/°C |
thermal conductivity | | ASTME1461 | 0.40到0.60 W/m/K |
| | ISO75-2/A | >200 °C |
| | ISO75-2/C | >170 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.