physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Antioxidant Additive??Antioxidant Additive ? 2?2 | 内部方法 | 0.030 到 0.10 % | |
Polystyrene Content | 内部方法 | 32 到 34 % | |
Total Extractables Total Extractables | 内部方法 | < 1.6 % | |
Volatile Matter | 内部方法 | < 0.50 % | |
内部方法 | 0.5 到 0.85 Pa·s |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore hardness | ASTM D2240 | 52 |
Elastic body | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile strength | 内部方法 | > 17.2 Mpa | |
内部方法 | 4.34 Mpa | ||
Tensile strain 3 | 内部方法 | > 800 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.