Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
ash content | 内部方法 | 0.40to0.65 % | |
density | ASTM D4025 | 0.940 g/cm³ | |
melt mass-flow rate | 10 g/10min | ||
Antioxidants | 内部方法 | 0.15to0.40 % | |
Polystyrene content | 内部方法 | 31to35 % | |
Total extractable substances | 内部方法 | <1.0 % | |
ash content | 4.0to6.0 % | ||
Volatile compounds | 内部方法 | <1.0 % | |
Solution viscosity | 内部方法 | 470to790 mPa·s |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore hardness | ASTM D2240 | 74 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
Content of diblock copolymer | 78.0 | ||
Styrene/rubber ratio | 33/67 |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ASTM D412 | 1.21 MPa | |
Yield | ASTM D412 | 1.72 MPa | |
elongation | Break | ASTM D412 | 600 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.