PA66 Razamid® A121 GR30

0
  • Properties:
    Filler
    glass fiber reinforced material
    30%
    filler by weight

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.37 g/cm³
Shrinkage rateASTMD9550.40到0.50 %
Mechanical propertiesTest ConditionTest MethodTest Result
Flexural modulusASTMD7909100 MPa
bending strengthASTMD790290 MPa
tensile strengthYieldASTMD638195 MPa
elongationBreakASTMD6384.0 %
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD25615 J/m
Electrical performanceTest ConditionTest MethodTest Result
Surface ResistivityIEC600931E+12 ohms
Volume resistivityIEC600931E+13 ohms·cm
Thermal performanceTest ConditionTest MethodTest Result
ASTMD648257 °C
ASTMD648255 °C
vicatASTMD1525240 °C
ASTMD3418260 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.