Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate | Equilibrium | ASTMD229 | 0.35 % |
density | | ASTMD792 | 1.80 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
Barcol Hardness | | | 48 |
flammability | Test Condition | Test Method | Test Result |
---|
FlameResistance | | ASTMD229 | 1.7 min |
UL flame retardant rating | | UL94 | HB |
FlameResistance | | ASTMD229 | 3.5 min |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
BondStrength | | ASTMD229 | 8.27 MPa |
Temperature Rating | | | 155 °C |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTMD638 | 75.8 MPa |
Flexural modulus | | ASTMD790 | 11000 MPa |
bending strength | | ASTMD790 | 172 MPa |
compressive strength | | ASTMD695 | 276 MPa |
shear strength | | ASTMD732 | 103 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 450 J/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|
dielectric strength | | ASTMD149 | 20 kV/mm |
dielectric constant | | ASTMD150 | 4.80 |
Dissipation Factor | | ASTMD150 | 0.020 |
arc resistance | | ASTMD495 | 150 sec |
Dielectric strength Step By Step InOil | | ASTMD149 | 60000 V |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.