EVA EVA PA-442

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO11830.950 g/cm³
melt mass-flow rateISO1133150 g/10min
Vinyl acetate content28.0 wt%
内部方法2.65 Pa·s
内部方法1.50 Pa·s
hardnessTest ConditionTest MethodTest Result
Shore AISO86874
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile stressBreakISO527-25.00 MPa
Tensile strainBreakISO527-2700 %
Thermal performanceTest ConditionTest MethodTest Result
melting temperature67.0 °C
RingandBall SoftningPointASTME2889 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.

Contact Us

Get App

Top