Polyester Sipolprene® 25170 W

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO1183,ASTMD7921.10 g/cm³
melt mass-flow rateASTMD1238,ISO113312 g/10min
Water absorption rate内部方法0.76 %
hardnessTest ConditionTest MethodTest Result
ASTMD2240,ISO86827
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD256无断裂
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthBreakASTMD638,ISO527-223.0 MPa
elongationBreakASTMD638,ISO527-2800 %
Flexural modulusASTMD790,ISO17830.0 MPa
abrasion resistanceDIN5351642.0 mm³
elastomerTest ConditionTest MethodTest Result
tear strengthASTMD100485.0 kN/m
Thermal performanceTest ConditionTest MethodTest Result
vicatISO306/A50,ASTMD1525273.0 °C
ASTMD3418,ISO3146173 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.